ASTM A333 tube Chemical Composition(%):
  Grade1 Grade3 Grade4 Grade6 Grade7 Grade8 Grade9 Grade10 Grade11
Carbon, max 0.3 0.19 0.12 0.3 0.19 0.13 0.2 0.2 0.1
Manganese 0.40-1.06 0.31-0.64 0.50-1.05 0.29-1.06 0.90 max 0.90 max 0.40-1.06 1.15-1.50 0.60 max
Phosphorus, max 0.025 0.025 0.025 0.025 0.025 0.025 0.025 0.035 0.025
Sulfur, max 0.025 0.025 0.025 0.025 0.025 0.025 0.015 0.025
Silicon 0.18-0.37 0.08-0.37 0.10 min 0.13-0.32 0.13-0.32 0.10-0.35 35.0-37.0
Nickel 3.18-3.82 0.47-0.98 2.03-2.57 8.40-9.60 1.60-2.24 0.25 max 0.50 max
Chromium 0.44-1.01 0.15 max 0.50 max
Copper 0.40-0.75 0.15 max
Aluminum 0.04-0.30 0.06 max
Vanadium, max 0.12
Columbium, max 0.05
Molybdenum, max 0.05 0.5 max
Cobalt 0.5 max
ASTM A333 tube Mechanical Properties:
  Grade 1 Grade 3 Grade 4 Grade 6 Grade 7 Grade 8
Psi MPa Psi MPa Psi MPa Psi MPa Psi MPa Psi
Tensile strength min 55000 380 65000 450 60000 415 60000 415 60000 450 100000
Yield strength min 30000 205 35000 240 35000 240 35000 240 35000 240 75000
Impact Temperature
Grade Minimum Impact Test Temperature
°F °C
1 -50 -45
3 -150 -100
4 -150 -100
6 -50 -45
7 -100 -75
8 -320 -195
9 -100 -75
10 -75 -60
ASTM A333 tube include seamless wall and welded carbon and steel pipe which are used at normal and low temperature circumstances. According to the temperature range it could be classified into grades from 1-7 or more.

ASTM A333 tube Grade and Temperature Test Chart:
Grade The lowest temperature for strike test
Grade 1 -50 -45
Grade 3 -150 -100
Grade 4 -150 -100
Grade 6 -50 -45
Grade 7 -100 -75
Grade 8 -320 -195
Grade 9 -100 -75
Grade 10 -75 -60